Abstract

The status of temperature-modulated differential scanning calorimetry is reviewed, including current methods of data analysis, and the experimental conditions and calibrations necessary for meaningful data interpretation. The theory and application of TMDSC to absolute heat capacity measurements, the glass transition, and crystallization and melting are also reviewed and discussed.