Laser engineered net shaping of nickel-based superalloy Inconel 718 powders onto AISI 4140 alloy steel substrates: interface bond and fracture failure mechanism

Hoyeol Kim, Weilong Cong, Hong-Chao Zhang, Z.C. Liu