Exergy Analysis of Atomic Layer Deposition for Al2O3 Nano-film Preparation

FenFen Wang, Tao Li, Hong-Chao Zhang, Chris Yuan

Research output: Contribution to conferencePaperpeer-review

Fingerprint

Dive into the research topics of 'Exergy Analysis of Atomic Layer Deposition for Al2O3 Nano-film Preparation'. Together they form a unique fingerprint.