Conversion of fullerenes to diamond under high pressure and high temperature

Yanzhang Ma, Guangtian Zou, Haibin Yang, Jinfang Meng

Research output: Contribution to journalArticle

19 Scopus citations

Abstract

Fullerenes have been converted to diamond crystals with the size of 0.1 mm at 5.0-5.5 GPa and 1400°C, using NiMnCo catalyst. They are similar to graphite in the growing phenomena. They are transformed into diamond directly without being graphitized first.

Original languageEnglish
Pages (from-to)822-823
Number of pages2
JournalApplied Physics Letters
Volume65
Issue number7
DOIs
StatePublished - 1994