Chemical and optical characterisation of atomic layer deposition aluminium doped ZnO films for photovoltaics by glow discharge optical emission spectrometry

S. W. Schmitt, Gerardo Gamez Goytia, V. Sivakov, M. Schubert, S. H. Christiansen, J. Michler

Research output: Contribution to journalArticle

Fingerprint Dive into the research topics of 'Chemical and optical characterisation of atomic layer deposition aluminium doped ZnO films for photovoltaics by glow discharge optical emission spectrometry'. Together they form a unique fingerprint.