Chemical and optical characterisation of atomic layer deposition aluminium doped ZnO films for photovoltaics by glow discharge optical emission spectrometry

S. W. Schmitt, G. Gamez, V. Sivakov, M. Schubert, S. H. Christiansen, J. Michler